MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Konson Lead Stearate for PVC Heat Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Name: Lead Stearate

CAS No: 1072-35-1

EC No:214-005-2

Linear molecular formula: [CH3(CH2)16COO]2Pb

Application: As an external lubricant, stabilizer in rigid and flexible plastic independently in some cases and generally with other lead stabilizers for high heat stability. In rigid plates and pipes In wire and cable jacketing As a paint drier in paint varnish and lacquer. It should be used in opaque products only since clarity

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 0.075 Mesh0.075 Meshmm mesh rate, >98%
 
Thermal PropertiesMetricEnglishComments
Melting Point 100 - 110 °C212 - 230 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Component Elements PropertiesMetricEnglishComments
Lead, Pb 26.5 - 28.5 %26.5 - 28.5 %
 
Descriptive Properties
Content<1%Free Fatty Acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS069 / 256114

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.