Eastar™ BR403 copolyester is a water-clear polymer that is great for toothbrush applications. It will not crystallize and thus offers wider processing latitude than conventional crystallizable polyesters while still providing an excellent combination of clarity, toughness, and melt strength. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.Information provided by Eastman. |