MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax Fiberfrax® LTC HSA™ Systems Ceramic Fiber Insulation
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® LTC HSA™ Systems is a ceramic fiber insulation constructed from multiple layers of ceramic fiber paper encapsulated between an outer covering of high-temperature woven textile cloth and parallel stitched to form a flexible insulation pad.

The thermal resistance properties exhibited by LTC HSA Systems are a result of the lightweight ceramic fiber paper core material composed of fine diameter fibers. This core paper has a small cell structure; in addition, all unfiberized particles have been eliminated. This results in very low thermal conductivity and good high-temperature insulation values. The high fiber index results in high resistance to mechanical and acoustical vibration. If wet by water or steam, all LTC HSA System's thermal and physical properties are restored upon drying. It also exhibits excellent chemical stability and resistance to attack from most corrosive agents. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies. Key performance features of LTC HSA Systems include:

  • Very low thermal conductivity
  • Lightweight
  • High-temperature insulating values
  • Excellent vibration resistance
  • Unaffected by moisture
  • Superior flexural integrity

Applications: The lightweight, excellent thermal and vibration resistance of LTC HSA Systems allow it to provide maximum insulating value while utilizing the least amount of weight and space. These features make LTC HSA Systems an idea choice for high-performance applications where critical areas are exposed to high operating temperatures, high vibration environments or are at risk from potential fire damage. Typical high-performance applications include:

  • Heat shield insulation on missiles, rockets and space exploration equipment
  • Thermal insulation on commercial and military aircraft - engine struts, thrust reversers, nacelles
  • Insulation liners for fire protection of hazardous material storage containers
  • Expansion joints for engine and turbine exhaust ducts

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00579 lb/in³Nominal Core Density
Loss On Ignition 1.03 %1.03 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1260 °C2300 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.50 %0.50 %
 
Descriptive Properties
Alumina-Silica Fibers (%)70
Glass Fiber (%)14
Inorganic Binder (%)2
Other (%)14
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber High Temperature Boards M Ceramic Fiber
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 3 hours
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator

CUNIF129 / 97901

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.