Notes: Monprene CP-33142 XRD1 is a clear, UV resistant thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-33142 XRD1 is a low hardness, low density grade that exhibits medium flow characteristics, suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Light Stabilized; Low Density; Lubricated; Low Specific Gravity; Low Hardness; Medium Flow; Slip; Sunlight Resistant; UV Absorbing; Without Fillers Uses: Consumer Applications; Gaskets; Handles; Toothbrush Handles; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |