MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BASF 3D Ultrafuse® PLA PRO1 Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Components: Polylactic acid based filament for Fused Filament Fabrication.

Product Description: PLA PRO1 is an extremely versatile tough PLA filament made for professionals. It reduces your printing time by 30% – 80%, (subject to printer and object limitations) and the strength exceeds overall mechanical properties of printed ABS parts. Printer settings can be tuned to achieve blazing fast speeds or an unrivaled surface finish. The excellent quality control ensures the highest levels of consistency between colors and batches, it will perform as expected, every time.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccPrinted Part; ISO 1183-1
Melt Flow 22.75 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 21.8 MPaZX: Upright; ISO 527
 48.0 MPaXY: Flat; ISO 527
Elongation at Break 0.90 %ZX: Upright; ISO 527
 21.9 %XY: Flat; ISO 527
Modulus of Elasticity 2.93 GPaYoung's, ZX: Upright; ISO 527
 3.166 GPaYoung's, XY: Flat; ISO 527
Flexural Strength 92.4 MPaXY: Flat; ISO 178
 99.1 MPaXZ: On its edge; ISO 178
Flexural Modulus 2340 MPaXZ: On its edge; ISO 178
 2823 MPaXY: Flat; ISO 178
Flexural Strain at Break 4.3 %XY: Flat; ISO 178
 4.4 %XZ: On its edge; ISO 178
Charpy Impact Unnotched 18.8 kJ/m²XZ: On its edge; ISO 179-2
 20.4 kJ/m²XY: Flat; ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 - 180 °CISO 11357-3
Glass Transition Temp, Tg 63.0 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 70.0 °CBed, Bed Material: Glass, tape at low temperatures
Nozzle Temperature 200 - 220 °C
Shelf Life 12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed40-150 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF3D003 / 312244

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.