MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ovako C45 5155 Steel, Quench & Tempering
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; AISI 1000 Series Steel

Material Notes: General Information: Grade SB-C45 is one of our carbon steel grades with a narrowed chemical composition in order to reach a high hardenability and it is also fine grain treated with Al. Grade 047A is an ingot casted low alloyed steel. High hardness and high strength can be achieved after hardening thanks to the relatively high carbon content. The steel is suitable for various type of applications where high strength is needed.

Information provided by Ovako

Key Words: C43, C44, C45R - 1.1201, C45E - 1.1191, Ck45, St70-2, SAE 1045, 080A42, SS 1672, XC 48, C 45, S 45 C, GOST 45, AISI/SAE/ASTM 1045
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 185 - 235
@Thickness 40.0 - 100 mm
Round bar
 190 - 240
@Thickness 25.0 - 40.0 mm
Round bar
Tensile Strength 630 - 780 MPa
@Thickness 40.0 - 100 mm
Round bar
 650 - 800 MPa
@Thickness 25.0 - 40.0 mm
Round bar
Tensile Strength, Yield >= 370 MPa
@Thickness 40.0 - 100 mm
Rel, Round bar
 >= 430 MPa
@Thickness 25.0 - 40.0 mm
Rel, Round bar
Elongation at Break 16 %
@Thickness 25.0 - 40.0 mm
Round bar
 17 %
@Thickness 40.0 - 100 mm
Round bar
Reduction of Area 40 %
@Thickness 25.0 - 40.0 mm
Round bar
 45 %
@Thickness 40.0 - 100 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 305 °CMS
 725 °CAC1
 760 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.44 - 0.49 %
Chromium, Cr <= 0.40 %
Iron, Fe 97.36 - 98.96 %As Balance
Manganese, Mn 0.50 - 0.80 %
Molybdenum, Mo <= 0.10 %
Nickel, Ni <= 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.10 - 0.40 %
Sulfur, S <= 0.025 %
 
Descriptive Properties
Dl1.1-1.8%
WeldabilityCEV 0.72max
 Pcm 0.55max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako S235JR SS 14 13 12:1987 (ref) Steel, +AR
Ovako C45 SB8673 Steel
EN S235JR Structural, Hot Rolled, Base Steel, 16 mm < t < 25 mm
Ovako C45 5081, Imatra 4 M Steel, +AR
EN S235JR High Manganese, Structural, Hot Rolled, Base Steel, t < 16 mm

NOVAKO388 / 234687

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.