MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek Poly-Optic® 1740 Urethane Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: Poly-Optic® 17-Series Urethane Resins are two-component, mercury-free, room temperature curing (RTV) systems that are formulated specifically for applications where optical clarity is a must. These polyurethane systems produce water-clear castings, but can be used in conjunction with PolyColor Dyes and dry fillers (e.g., fine metal powders) to create a myriad of effects. Poly-Optic resins are the plastics of choice for mimicking glass and ice-like features and are widely used to create stunning prototypes (lenses, bottles, containers), as well as unique art, medical models, sculpture and display items. Vacuum and/or pressure casting techniques are recommended for bubble-free parts..

Product Line Features:

  • Non-Mercury Formulas
  • Water clear
  • Reproduces fine detail
  • Can be machined, drilled and sanded
  • Low shrinkage upon cure
  • Low Viscosity
  • Easily accepts PolyColor Dyes and dry fillers

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
Viscosity 400 cP400 cPMixed
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
Tensile Strength 21.9 MPa3180 psi
Elongation at Break 12 %12 %
Modulus of Elasticity 0.552 GPa80.1 ksi
Flexural Strength 24.5 MPa
@Strain 5.0 %
3560 psi
@Strain 5.0 %
Flexural Modulus 0.627 GPa91.0 ksi
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 58.3 °C137 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourDemold Time
Pot Life 14.0 min14.0 min
 
Descriptive Properties
Cured ColorWater Clear
Maximum Exotherm210°F
Mix Ratio By Weight1A:1B
Specific Volume28.5 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5075 / 251067

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.