MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M 8418 Polyester Film Tape
Categories: Polymer; Adhesive; Film

Material Notes: 3M™ Polyester Film Tape 8417 is a self-wound (linerless) transparent polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. It is often used as an overlaminate in conjunction with 3M™ Polyester Film Tape 8418. 3M™ Polyester Film Tape 8418 is a white polyester film coated with 3M Adhesive 100 High-temperature Acrylic and has a liner.

Features:

  • Adheres instantly to a variety of surfaces.
  • Tough film backing resists edge tear when processing and dispensing.
  • Non-corrosive and chemical resistant.
  • High and low temperature stability.
  • 3M polyester film tape 8418 is printable with common processes and inks.
  • 3M polyester film tape 8417 provides good transparency when used as an overlaminate.
  • When used together, the tapes pass all requirements for Federal Specification MIL-T-100B, Amendment 1 for non-corrosive, heat, cold and solvent-resistant identification tape.
Applications:
  • Fluid-line identification.
  • General identification applications where chemical and temperature resistance is desired.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milFacestock
 30.5 microns1.20 milAdhesive
 55.9 microns2.20 milTotal
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 100 %100 %
Peel Strength 0.1643 kN/m0.9375 pliPolypropylene, 180° Peel, 10 min dwell; ASTM D3330
 0.27391 kN/m1.5625 pliABS, 180° Peel, 10 min dwell; ASTM D3330
 0.36156 kN/m2.0625 pliStainless Steel, 180° Peel, 10 min dwell; ASTM D3330
 0.4163 kN/m2.375 pliGlass, 180° Peel, 10 min dwell; ASTM D3330
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Adhesive Type100 High-temperature Acrylic)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33460 / 168207

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.