MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 24946DN-1 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24946DN-1 is a high performance thermoplastic vulcanizate use in automotive applications. This grade is a high hardness, lubricated grade exhibiting sunlight resistance and UV absorbing characteristics. This grade can be processed by injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; High Hardness; Light Stabilized; Low Density; Low Flow; Low Specific Gravity; Lubricated; Slip; Sunlight Resistant; UV Absorbing

Uses: Expansion Joint; Gaskets; Glazing; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccISO 1183
Viscosity 342 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Apparent; ASTM D3835
Melt Flow 4.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 44
@Time 15.0 sec
Injection Molded; ISO 868
 45
@Time 5.00 sec
Injection Molded; ISO 868
 47
@Time 1.00 sec
Injection Molded; ISO 868
 45
@Treatment Temp. 125 °C,
Time 5.00 sec
Injection Molded, Change in Air, 168; ISO 888
 47.2
@Treatment Temp. 110 °C,
Time 15.0 sec
Injection Molded, Change in Air, 1008; ISO 888
 48.2
@Treatment Temp. 110 °C,
Time 5.00 sec
Injection Molded, Change in Air, 1008; ISO 888
 49.2
@Treatment Temp. 125 °C,
Time 15.0 sec
Injection Molded, Change in Air, 168; ISO 888
 49.9
@Treatment Temp. 110 °C,
Time 1.00 sec
Injection Molded, Change in Air, 1008; ISO 888
 51.5
@Treatment Temp. 125 °C,
Time 1.00 sec
Injection Molded, Change in Air, 168; ISO 888
Tensile Strength at Break 1550 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1990 psiFlow, Type 1, 20 in/min; ISO 37
 1430 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 1570 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 2230 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 2570 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 1260 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 1820 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 1420 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air in 1008 hr; ISO 188
 1470 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air in 168 hr; ISO 188
 2240 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air in 1008 hr; ISO 188
 2570 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air in 168 hr; ISO 188
Elongation at Break 480 %Flow, Type 1, 20 in/min; ISO 37
 590 %Across Flow, Type 1, 20 in/min; ISO 37
 230 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 245 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 301 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 325 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 360 pliMethod Ba, Angle (Unnicked), Flow, 20 in/min; ISO 34-1
 730 pliMethod Ba, Angle (Unnicked), Across Flow, 20 in/min; ISO 34-1
Compression Set 39 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 64 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 78 %
@Temperature 90.0 °C,
Time 252000 sec
Type A; ISO 815
 98 %
@Temperature 125 °C,
Time 252000 sec
Type A; ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 374 - 446 °FInjection, Melt
Rear Barrel Temperature 344 - 416 °FInjection
Middle Barrel Temperature 354 - 426 °FInjection
Front Barrel Temperature 364 - 436 °FInjection
Nozzle Temperature 374 - 446 °FInjection
Zone 1 330 - 400 °FExtrusion
Zone 2 340 - 410 °FExtrusion
Zone 3 350 - 420 °FExtrusion
Zone 4 355 - 425 °FExtrusion
Zone 5 360 - 430 °FExtrusion
Die Temperature 374 - 440 °FExtrusion
Mold Temperature 95.0 - 140 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1199 / 237690

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.