MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duracon® CH-15 CD3501 Acetal Copolymer, CF
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: Electric conductive. 15% carbon fiber reinforced. Low wear.

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Filler Content 15 %15 %Carbon fiber
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 2.00 mm
0.0060 in/in
@Thickness 0.0787 in
Cavity pressure 60 MPa; 60x60x2; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
0.010 in/in
@Thickness 0.0787 in
Cavity pressure 60 Mpa; 60x60x2; ISO 294-4
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 130 MPa18900 psiISO 527-1,2
Elongation at Break 1.5 %1.5 %ISO 527-1,2
Tensile Modulus 11.7 GPa1700 ksiISO 527-1,2
Flexural Strength 185 MPa26800 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179/1eA
Coefficient of Friction, Dynamic  0.27
@Pressure 0.490 MPa
0.27
@Pressure 71.1 psi
Thrust, vs C-Steel. 30 cm/s; JIS K7218
 0.37
@Pressure 0.0600 MPa
0.37
@Pressure 8.70 psi
Thrust, vs M90-44. 15 cm/s; JIS K7218
K (wear) Factor  10.0 x 10-8 mm³/N-M
@Pressure 0.490 MPa
4.96 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, steel side. 30 cm/s; JIS K7218
 200 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
99.3 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, material side. 15 cm/s; JIS K7218
 500 x 10-8 mm³/N-M
@Pressure 0.490 MPa
248 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, material side. 30 cm/s; JIS K7218
 10000 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
4960 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, M90-44 side. 15 cm/s; JIS K7218
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 ohm-cm1000 ohm-cmStandard test
Surface Resistance 300 ohm300 ohmStandard test
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
5.56 µin/in-°F
@Temperature 73.4 - 131 °F
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9820 / 305493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.