MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® Nature Range NR-M49 Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Viscosity  1000 cP
@Temperature 120 °C
1000 cP
@Temperature 248 °F
Rheology (EN6043-A, 2°C/min)
 40000 cP
@Temperature 40.0 °C
40000 cP
@Temperature 104 °F
Rheology (EN6043-A, 2°C/min)
 1.00e+8 cP
@Temperature 150 °C
1.00e+8 cP
@Temperature 302 °F
Rheology (EN6043-A, 2°C/min)
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 80.0 °C176 °Fonset wet
 105 °C221 °Fonset dry
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 140 °C
0.500 hour
@Temperature 284 °F
 60.0 min
@Temperature 120 °C
1.00 hour
@Temperature 248 °F
 120 min
@Temperature 100 °C
2.00 hour
@Temperature 212 °F
normal
 318 min
@Temperature 90.0 °C
5.30 hour
@Temperature 194 °F
 720 min
@Temperature 85.0 °C
12.0 hour
@Temperature 185 °F
Gel Time  11.0 min
@Temperature 140 °C
11.0 min
@Temperature 284 °F
 19.0 min
@Temperature 130 °C
19.0 min
@Temperature 266 °F
 31.0 min
@Temperature 120 °C
31.0 min
@Temperature 248 °F
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9139 / 322295

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.