MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Rohaglas® 99524 Clear Acrylic Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes: ROHAGLAS® Film 99524 acrylic film, based upon polymethyl methacrylate and acrylic elastomers, offers crystal-clear optical properties with two glossy (Class A) surfaces. Its excellent abrasion resistance, combined with long-term outdoor weatherability offers outstanding performance as a decor carrier and as a substrate surface protector. ROHAGLAS 99524 film has superior processability in die-cutting and all forming processes. In addition, it presents good resistance towards weak acids and alkalis as well as non-polar solvents.

Information provided by Cyro Industries

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 54.0 MPaISO 527
Elongation at Break 35 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 2.20 GPaISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 250
Surface Resistance >= 1.00e+13 ohmIEC 250
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 250
 0.050
@Frequency 100 Hz
IEC 250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
DIN 53752A
Specific Heat Capacity 1.50 J/g-°C
Thermal Conductivity 0.190 W/m-K
Vicat Softening Point 100 °CB/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489
Haze <= 0.60 %ASTM D1003
Yellow Index <= 0.40 %ASTM D1925
Transmission, Visible 92 %DIN 5036
UV Transmittance <= 0.20 %
@Wavelength 280 - 380 nm
DIN 5036
 
Descriptive Properties
Birefringence ASTM D4093max 20 nm
Pencil Hardness2ASTM D3363
Weather Resistance, Xenotest 1200/5000hrno change

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Acrylic Film
Röhm Acrylite® 249 Acrylic Sheet, Aerospace Grade
Röhm Acrylite® GMS Acrylic Sheet, Aerospace Grade
Röhm PLEXIGLAS® Film 0F043 PMMA
Evonik DEGALAN® 4140 D Methacrylic Polymer

PCYRO02 / 29179

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.