TRA-GREASE GFC-F1 is a silicone based thermal grease. This product provides extremely low thermal resistance. It is designed to provide heat dissipation in processors and high power devices. Typical applications include providing maximum heat transfer between an active device and a heat spreader or heat sink. Information provided by Tra-Con Inc. |