MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and NSF compliant and holds its excellent mechanical properties over a wide range of temperatures.

Uses: ENSIFONE 's unique combination of chemical and hydrolytic resistance, high-temperature performance, good mechanical properties, and agency approvals make it an excellent choice for applications in the pharmaceutical, medical, food service equipment, semiconductor processing, and electronic equipment industries.

Ensifone grades have been replaced by Tecason

Information supplied by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.30 %24 hrs.; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Ultimate 69.8 MPaASTM D638
Elongation at Break 50 - 100 %ASTM D638
Tensile Modulus 360000 psiASTM D638
Flexural Yield Strength 106.2 MPaASTM D790
Flexural Modulus, 1% Secant 2.70 GPaASTM D790
Izod Impact, Notched 0.690 J/cmASTM D256
Coefficient of Friction, Dynamic 0.3740 psi, 50 fpm; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 5.00e+16 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 16.5 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.8 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Maximum Service Temperature, Air 141 °CLong Term
 171 °CShort Term
Deflection Temperature at 0.46 MPa (66 psi) 181 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 174 °CASTM D648
Flammability, UL94 V-0
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphorus (V) Sulfide Trifluoride, PSF3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
BASF Ultrason® S 2010 PSU
Solvay FM® 300-2K Film Adhesive, psf 0.1 (489 gsm)
Trinseo Magnum™ 4435 ABS

PENS03 / 35972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.