MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3003/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Liquid silicone rubbers of the ELASTOSIL® LR 3003 series are paste-like, easily-pigmentable two component compounds with short curing times. Their vulcanizates are noted for their high transparency and excellent mechanical and electrical properties.

Properties: Narrow Shore hardness range from 38 to 44 Shore A (41 ± 3 Shore A). The products can be used within a temperature range of - 55 °C to + 210 °C. The addition of heat stabilizers at service temperatures of more than 180 °C is recommended.

Application: These grades are particularly suitable for the economical production of large series of injection molded articles. Parts made from ELASTOSIL® LR 3003/40 A/B can be used for technical applications. These articles are also suitable for use in conjunction with foodstuffs. Postcured parts can be used for food contact applications and are suitable for use under the Recommendation "XV. Silicones" of the BfR and FDA § 177.2600 under observance of any given limitations on extractable and volatile substances.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDIN EN ISO 1183-1 A
Viscosity 420000 cP
@Shear Rate 10.0 1/s
DIN 53019
 840000 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 41DIN 53505
Tensile Strength at Break 10.0 MPaDIN 53504 S 1
Elongation at Break 610 %DIN 53504 S 1
Rebound 57 %DIN 53512
Tear Strength 188 pliASTM 624 B
Compression Set 13 %
@Temperature 175 °C,
Time 79200 sec
post cure 6h/200°C; DIN ISO 815-B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+15 ohm-cmDIN IEC 93
Dielectric Constant 2.8
@Frequency 50 Hz
DIN VDE 0303
Dielectric Strength 23.0 kV/mm
@Thickness 1.00 mm
DIN IEC 243-2
Dissipation Factor 0.00020
@Frequency 50 Hz
DIN VDE 0303
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °Cwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
in press, postcuring for 4h/200°C (in ventilated air)
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
Wacker Elastosil® LR 3003/30 A/B Liquid Silicone Rubber
Seals Eastern 5803 Fluoro-silicone
Wacker Elastosil® FLR 3900/40 A/B Liquid Fluorosilicone Rubber
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber

PWACK9090 / 204619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.