MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Colour Image Plastic Compound Electroblend® PP-1804 PP
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Electroblend® PP-1804 is a conductive polypropylene compound characterized by medium flow rate.

Features:

  • Conductive
  • Medium flow
  • Excellent thermal & mechanical properties
Uses:
  • Automotive applications
  • Industrial parts
  • Electronic & Electrical parts
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.0 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 41.0 MPaASTM D790
Flexural Modulus 1230 MPaASTM D790
Izod Impact, Notched 132 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 ohm - 1e+05ASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
@Thickness 4.00 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 185 - 190 °C
Middle Barrel Temperature 190 - 195 °C
Front Barrel Temperature 195 - 210 °C
Nozzle Temperature 210 - 220 °C
Melt Temperature 190 - 220 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 hour
 <= 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLO086 / 265978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.