MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EFI Composites Featherlite FL4005A Aluminum Trihydrate/Thermoplastic Microspheres
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Featherlite FL4005A is a concentrated blends of thermoplastic microspheres and alumina tri-hydrate combined with an effective dust suppressant. Alumina Tri-Hydrate based light weight concentrate (density .5 g/cc) for improved flame suppression. Compatible with almost any resin system where flame suppression and weight reduction is important. These low dust blends are designed to be used in areas where dust sensitivity is a priority while improving product wet out and lowering resin demand. The alumina tri-hydrate filler offers increased flame suppression and is less reactive with acidic chemicals and resins than other heavy fillers.

Key Words: AL(OH)3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0500 g/cc0.0500 g/cc
Moisture Absorption <= 0.100 %<= 0.100 %
Particle Size 80 µm80 µmMean
pH 7.87.8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 27.3 %27.3 %Bound
 
Descriptive Properties
ColorOff White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DWA 6091/SiC/20p-T6 Aluminum SiC Metal-Matrix-Composite (Al MMC)
Zircar Refractory Composites RS-99-45 Refractory Sheet
Zircar Refractory Composites RS-A3 Refractory Sheet
Zircar Refractory Composites RS-99-60 Refractory Sheet
DWA 2009/SiC/25p-T4 Aluminum SiC Metal-Matrix-Composite (Al MMC)

EEFI990 / 230551

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.