MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) HIPS 8350 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: HIPS 8350 is a very high impact polystyrene used in the extrusion industry. This grade has an improved environmental stress crack resistance (ESCR) in comparison with standard high impact polystyrene grades. It is recommended for the production of packaging intended for products likely to cause stress cracking. HIPS8350 retains good mechanical properties at low temperatures making this grade suitable for frozen food packaging and for the production of fridge liners in contact with HCFC expanded foam insulation.

Applications: extrusion sheet for thermoforming, fridge doors and cabinet liners

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Moisture Absorption <= 0.100 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D570
Melt Flow 4.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPaASTM D638
Tensile Strength, Yield 18.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 1600 MPaASTM D638
Flexural Modulus 1600 MPaASTM D790
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 92.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene
Iran Petrochemical (PCC) Arak I4 HDPE
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene

PIPC342 / 149776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.