MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds EPSILON® Hardener: 102 Medium Thixotropic epoxy coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Epoxy

Material Notes: Product Overview: EPSILON™ is a thixotropic epoxy coating that self thickens for brushing onto a variety of surfaces without sagging. Parts A and B mix together easily, and the mixture wets out uniformly. This product is not sensitive to moisture or humidity. EPSILON™ cures at room temperature to an impact resistant plastic which exhibits good compressive and flexural strength. EPSILON™ is color neutral, and cured material can be easily sanded, primed and painted. EPSILON™ is suitable for use as a protective, impact resistant coating for EPS or polyurethane foam. It can also be applied to plaster, concrete, wood and fabrics. This product is not sensitive to moisture or humidity and contains no VOC’s.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D-1475
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D-2240
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min2.00 hourThin Film Working Time
 180 min3.00 hourThin Film Tacky Recoat Time
 300 min5.00 hourThin Film, Tack Free Time
 1440 min24.0 hour
Pot Life 30.0 min30.0 minASTM D-2471
 
Descriptive Properties
ColorBeige
Mix Ratio100A:20Bby weight
Mixed ViscosityVariable
Specific Volume24.3[in3/lb]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN205 / 296906

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.