MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmoderm® 43191 Granular Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Desmoderm 43191 Granular is a one-component polyester polyether urethane based on an aromatic diisocyanate.

Uses: Desmoderm 43191 Granular is used as the flexible component in the polyurethane coagulation process. Desmoderm 43191 Granular is suitable for use in the manufacture of materials for shoe linings, shoe uppers, clothing and bags/luggage.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 4000 - 20000 cP4000 - 20000 cPUntempered; DIN EN ISO 3219/A.3
 4000 - 40000 cP4000 - 40000 cPTempered, 5 h, 120°C; DIN EN ISO 3219/A.3
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 - 40.0 MPa4350 - 5800 psiDIN 53504
 25.0 - 35.0 MPa
@Temperature 70.0 °C
3630 - 5080 psi
@Temperature 158 °F
after 14 d hydrolysis, 95% RH; DIN 53504
Elongation at Break 650 - 750 %650 - 750 %DIN 53504
100% Modulus 4.00 MPa
@Strain 100 %
580 psi
@Strain 100 %
DIN 53504
 
Thermal PropertiesMetricEnglishComments
Softening Point 190 - 200 °C374 - 392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
Covestro Texin® 4215 Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 1045D TPU
Covestro Desmomelt® 530 Polyurethane
Covestro DESMODURE® N 100A Polyurethane

PCOVEST0294 / 202077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.