MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Torlon® 4645 PAI, Excellent wear resistance in lubricated environments
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: Excellent wear resistance in lubricated environments, contains PTFE and carbon fiber

Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep and chemicals.

Potential applications for Torlon® 4645 polyamide-imide include thrust washers, seal rings, sliding vanes, bobbins, bushings, clutch rollers and pistons.

Markets/Uses: Automotive / Drivetrain / Lubricated; Automotive / Drivetrain / Needle Bearing Replacement Rings; Automotive / Drivetrain / Seal Rings; Automotive / Drivetrain / Thrust Bearings; Automotive / Drivetrain / Thrust Washers; Wear-Resistant Plastics / High Temperature Friction & Wear / Lubricated

Applications: Automotive Applications; Bearings; Bobbins; Bushings; Seals; Thrust Washer

Features: Chemical Resistant; Creep Resistant; Flame Retardant; High Heat Resistance; High Stiffness; High Temperature Strength; Low Friction; Self Lubricating; Semi Conductive; Wear Resistant

Injection notes: Minimum drying times are: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio between 1:1 and 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors: Drake extrudes shapes and machines and injection molds parts in Torlon® PAI, PEEK, PAEK, Ryton PPS and Ultem PEI. It also machines Vespel® PI. Innovations include cryogenic CryoDyn® CT-200 shapes as a PCTFE alternative; efficient Seamless Tube® and the largest extruded rod diameters to >254mm and plate thicknesses to > 100mm. Certified to ISO 9001:2015 and AS9100D. Visit www.DrakePlastics.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccASTM D792
Water Absorption 0.25 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 114 MPaASTM D638
Elongation at Break 0.80 %ASTM D638
Tensile Modulus 18600 MPaASTM D638
Flexural Strength 154 MPaASTM D790
Flexural Modulus 12400 MPaASTM D790
Compressive Strength 157 MPaASTM D695
Shear Strength 60.7 MPa
@Temperature 150 °C
ASTM D732
 85.5 MPa
@Temperature 23.0 °C
ASTM D732
Izod Impact, Notched 37.0 J/mASTM D256
Izod Impact, Unnotched 110 J/mASTM D256
Coefficient of Friction 0.070 - 0.090ASTM D1894
K (wear) Factor 0.300 x 10-10 in³-min/ft-lb-hrASTM D3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 281 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 °C
Nozzle Temperature 371 °C
Mold Temperature 199 - 216 °C
Drying Temperature 177 °C
@Time 10800 sec
Moisture Content <= 0.050 %Injection
Back Pressure 6.89 MPa
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AdditiveCarbon Fiber + PTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4550 / 280350

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.