MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vinnolit® E 68 CT PVC for Plastisol Preparation
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® E 68 CT PVC for plastisol preparation. Vinnolit® E 68 CT is an E-PVC homopolymer which is readily converted into plastisols of very low viscosity and good shelf life, even at high filler loads. It exhibits no flow anomalies like dilatancy, even at high shear rates (processing window) where it shows low viscosities as well. Foams based on Vinnolit® E 68 CT yield matt films of very high whiteness and with foam structures ideal for hot embossment. Fast Foam height development and high gelling speed are also characteristic for Vinnolit® E 68 CT. Main application of Vinnolit® E 68 CT are hot embossed wallcoverings, but it may also be applied for all common artificial leather and all other applications requiring foams of very high whiteness.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %ISO 1269
Particle Size <= 63 µm<= 63 µm<= 1.0% Retained on 0.063 mm Sieve; DIN EN ISO 53195
Viscosity  3600 cP
@Shear Rate 400 1/s
3600 cP
@Shear Rate 400 1/s
100:60 in DINP; ISO 1060-2 11468
 4390 cP
@Shear Rate 2.50 1/s
4390 cP
@Shear Rate 2.50 1/s
100:60 in DINP; ISO 1060-2 11468
Viscosity Test 116 cm³/g1.16 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentMedium
K-Value68ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINNO947 / 291144

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.