MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB SCANAMID 66 A12^ F25 NH10 Nylon 66, Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes:

Information provided by Polykemi AB

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ISO 1183
Filler Content 25 %25 %±2%; Polykemi
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus 8.50 GPa
@Temperature 23.0 °C
1230 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 249 °C480 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 233 °C451 °F120°C/h; ISO 75/1
Vicat Softening Point  226 °C
@Load 5.001 kg
439 °F
@Load 11.03 lb
50°C/h; ISO 306
 248 °C
@Load 1.00 kg
478 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
Glow Wire Test 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYK056 / 122781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.