MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovation Polymers OpteSTAT™ NC TPU 9020 Polyurethane-based Carbon Nanotube Compound
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Carbon Fiber Reinforced

Material Notes: Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or other electronic assemblies where ESD control is required while retaining exceptional cleanliness, dimensional control and physical properties

All properties after 48hrs conditioning at 23°C/50% RH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7.00 MPa50 mm/min; ASTM D638
Elongation at Yield 6.5 %50 mm/min; ASTM D638
Izod Impact, Notched 0.900 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 10000 - 1.00e+7 ohmASTM D257

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers Nima™ NH PC143P Polycarbonate
Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced
Ovation Polymers Nemcon™ H PA DP117/X3 Polyphthalamide, Thermally Conductive
Ovation Polymers Nemcon™ H PC DP111/X1 Polycarbonate

POVAT145 / 79124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.