MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMOPHEN® 1200 BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Slightly branched, hydroxyl-bearing polyester. In the formulation of flexible polyurethane coatings.

Properties / Applications: Clear and pigmented combinations of Desmophen® 1200 BA and more highly branched Desmophen® grades are reacted with Desmodur® L, HL and IL to formulate coatings for substrates such as metal, wood and various plastics. When combined with Desmophen® 1700, Desmophen® 1200 BA can be used to formulate coatings for flexible substrates such as rubber.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccDIN 51757
Volatiles 39 - 41 %(2 g resin/2ml toluene/1 h/125 °C/convection oven); DIN EN ISO 3251
Viscosity 55 cPDIN EN ISO 3219
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 2.5[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Flash Point 34.0 °CDIN 53213/1
 
Processing PropertiesOriginal ValueComments
Moisture Content >= 0.10 %DIN 51 777/1
 
Descriptive Properties
Color<130Hazen, DIN EN 1557
Content2.8-3.2%Hydroxyl, DIN 53 240/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNACOLL® 7130 Copolyester
Evonik DYNACOLL® 7380 Copolyester
Syensqo (Solvay Specialty Polymers) Ixef® 2060 Polyarylamide (PARA)
Covestro DESMOPHEN® 651 MPA Polyurethane
Covestro DESMOPHEN® 650A-65 PMA Polyurethane

PCOVEST0739 / 202522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.