MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

GEHR Plastics PEEK-30CF® Polyetheretherketone, 30% carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

information provided by GEHR

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccISO 1183
Moisture Absorption at Equilibrium 0.16 %0.16 %ISO 62
Water Absorption at Saturation 0.35 %0.35 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ISO 2039
Hardness, Shore D 9292ISO 868
Ball Indentation Hardness 312 MPa45300 psiISO 2039
Tensile Strength at Break 122 MPa17700 psiISO 527
Tensile Strength, Yield 122 MPa17700 psiISO 527
Elongation at Break 7.0 %7.0 %ISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Modulus of Elasticity 6.80 GPa986 ksiISO 527
Flexural Strength 193 MPa28000 psiISO 178
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+05<= 1e+05IEC 60093
Surface Resistance <= 1e+05<= 1e+05IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FISO 11359
Thermal Conductivity 0.900 W/m-K
@Temperature 20.0 °C
6.25 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
ISO 22007-4
Melting Point 343 °C649 °FDIN EN ISO 3146
Maximum Service Temperature, Air 260 °C500 °FUL 746B
Deflection Temperature at 1.8 MPa (264 psi) 336 °C637 °FISO 75
Minimum Service Temperature, Air -20.0 °C-4.00 °FUL 746B
Glass Transition Temp, Tg 143 °C289 °FDIN EN ISO 3146
Flammability, UL94 V-0V-0UL 94
Oxygen Index 40 %40 %ASTM D2863
 
Compliance PropertiesMetricEnglishComments
FDA NoNoPhysiological indifference
 
Descriptive Properties
Bondabilityyes
Colorblack
Physiological indifferenceno, EEC
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAKEEP® 2000 CF30 PEEK
Akro-Plastic Akrotek® PEEK CF 30 black (5049) PEEK, Dry, 30% Carbon Filled
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced

PGEHR039c / 192464

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.