MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical GOYENCHEM-TXFT Impregnation Treatment Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GOYENCHEM-TXFT is high effective synthetic nanometer construction product. It has excellent flame retardant ability and good water solubility. GYC provides complete solution project to the problem of “ durability” and “ water-resistant” for flame retardant fiber. GOYENCHEM-TXFT, pioneer permanent flame retardant technique, can be applied into construction decoration, high value flame retardant curtain, interior fabric for auto industry, curtain, special working clothes…etc. It’s suitable for synthetic fiber, polyester, T/C blending, artificial fiber, flame retardant for PU coating fabric…etc. Textiles treated with GOYENCHEM-TXFT can have permanent and wash resistant flame retardant ability and can be comprehensive applied.

Applications:

  • Thermosetting resin: Phenolic resin, acrylic, epoxy, unsaturated binding resin, a polyester resin, an acrylic resin ….. etc
  • Coating and comprehensive resin: fireproof coating, all kinds of related acrylic products, PU, PMMA, latex resins, adhesives related products
  • Thermoplastic fields: TPU, TVE, PP, POLYOLIFIN, PET, NYLON, POM, engineering plastic.
  • Rubber industires: EPDM, CR, NBR, SBR, SIR, CSM, NR, IIR and various flame retard rubber.
  • Elastomers: TPE, TPU, SBS, SEBS, TPR, TPV and all kinds of elastomers.
  • Foaming polymer: GOYENCHEM-TXFT can be applied on several compound foaming products, especially on flexible and rigid PU, EVA foaming material, EPS foaming.
  • Other application: printing ink, paper industires, furniture plywood, pigment, back glue, masterbatch, textile and all kinds of electronic products.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.30 g/cc0.0434 - 0.0470 lb/in³
Particle Size 5.0 - 10 µm5.0 - 10 µm
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 5.0<= 5.0mgKOH/g
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40
 
Descriptive Properties
AppearanceLiquid
ColorTransparent yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN202 / 266510

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.