MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC XENOY™ 1760E PC+PBT (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of XENOY 1760 resin.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Density 1.30 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 27 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 84.0 MPa5 mm/min; ISO 527
 84.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 84.0 MPa5 mm/min; ISO 527
 84.0 MPa5 mm/min; ASTM D638
Elongation at Break 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Tensile Modulus 4800 MPa1mm/min; ISO 527
 5310 MPa5 mm/min; ASTM D638
Flexural Yield Strength 131 MPa1.3 mm/min, 50 mm span; ASTM D790
 133 MPa2 mm/min; ISO 178
Flexural Modulus 3910 MPa1.3 mm/min, 50 mm span; ASTM D790
 4010 MPa2 mm/min; ISO 178
Izod Impact, Notched 63.0 J/mASTM D256
 60.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 3.00 kJ/m²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 12.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 8.00 JASTM D3763
 3.00 J
@Temperature -30.0 °C
peak; ASTM D3763
 3.00 J
@Temperature -30.0 °C
ASTM D3763
 4.00 J
@Temperature -20.0 °C
peak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 39.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 39.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 101 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 116 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 121 °CRate B/50; ASTM D1525
 130 °CRate B/120; ISO 306
 135 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 275 °CInjection Molding
Zone 1 250 - 270 °C
Zone 2 255 - 275 °C
Zone 3 260 - 280 °C
Melt Temperature 260 - 280 °C
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.600 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10820 / 244287

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.