MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC VALOX™ SHF4340 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 20% GF Super High Flow PBT

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³ISO 1183
Water Absorption 0.15 %0.15 %23°C/sat; ISO 62
Moisture Absorption 0.0300 %0.0300 %23°C / 50% RH; ISO 62
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 250 °C
40 g/10 min
@Load 4.76 lb,
Temperature 482 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psi5 mm/min; ISO 527
Tensile Strength, Yield 110 MPa16000 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 6.70 GPa972 ksi1mm/min; ISO 527
Flexural Yield Strength 145 MPa21000 psi2 mm/min; ISO 178
Flexural Modulus 5.60 GPa812 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 38.0 kJ/m²18.1 ft-lb/in²80*10*4; ISO 180/1U
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
22.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 204 °C399 °FRate B/50; ISO 306
 204 °C399 °FRate B/120; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature
Nozzle Temperature 240 - 260 °C464 - 500 °FInjection Molding
Zone 1 230 - 245 °C446 - 473 °F
Zone 2 240 - 255 °C464 - 491 °F
Zone 3 245 - 265 °C473 - 509 °F
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 40.0 - 100 °C104 - 212 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10290 / 243757

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.