Topilene ® J440F is a specially designed polypropylene block copolymer that features high impact strength and excellent optical properties. It is suitable for protective CPP film extrusion. Topilene® J440F complies with FDA 21 CFR 177.1520 and EU No 10/2011 for food contact. Typical Applications: Protective CPP film for IT industries / Cast Film Features: High Impact Strength / Excellent Optical Properties / Very Low Fisheye / Medium Haze /Good Heat Resistance / Enhanced Processability |