MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
General Plastics LAST-A-FOAM® TR-15 Polyurethane Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:

Information provided by General Plastics Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.240 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 26.1ASTM D2240
Tensile Strength 479 psiPerpendicular to Rise; ASTM D1623
 514 psiParallel to Rise; ASTM D1623
Tensile Modulus 23477 psiPerpendicular to Rise; ASTM D1623
 31206 psiParallel to Rise; ASTM D1623
Flexural Strength 677 psiRise Parallel to Beam Thick.; ASTM D790
 690 psiRise Parallel to Test Span; ASTM D790
Flexural Modulus 23620 psiRise Parallel to Beam Thick.; ASTM D790
 24616 psiRise Parallel to Test Span; ASTM D790
Compressive Strength 444 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 470 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 623 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
 627 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 925 psi
@Temperature -51.1 °C
Perpendicular to Rise; ASTM D1621
 955 psi
@Temperature -51.1 °C
Parallel to Rise; ASTM D1621
Compressive Modulus 13049 psi
@Temperature 71.1 °C
Perpendicular to Rise; ASTM D1621
 16028 psi
@Temperature 71.1 °C
Parallel to Rise; ASTM D1621
 17240 psi
@Temperature 23.9 °C
Perpendicular to Rise; ASTM D1621
 18967 psi
@Temperature -51.1 °C
Perpendicular to Rise; ASTM D1621
 21524 psi
@Temperature -51.1 °C
Parallel to Rise; ASTM D1621
 22132 psi
@Temperature 23.9 °C
Parallel to Rise; ASTM D1621
Poissons Ratio 0.30
Shear Modulus 6.809 ksiRise Parallel to Specimen Length; ASTM C273
 6.874 ksiRise Parallel to Specimen Thickness; ASTM C273
Shear Strength 0.419 ksiRise Parallel to Specimen Length; ASTM C273
 0.421 ksiRise Parallel to Specimen Thickness; ASTM C273
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µin/in-°F
@Temperature -28.9 - 71.1 °C
GP Method
Thermal Conductivity 0.321 BTU-in/hr-ft²-°FASTM C518
Glass Transition Temp, Tg 256 °FASTM E1824
 
Descriptive Properties
Closed Cell Content96.9%ASTM D2856 Procedure B
Tumbling Friability (%)4.220 mins at 60 rpm, ASTM C421

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carlisle 201HD Carbon-Carbon Composite
Covestro Bayfill® EA 2001 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
General Plastics LAST-A-FOAM® FR-10106 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-10108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-7105 Polyurethane Foam

PGENR069 / 186855

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.