MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC SABIC® Vestolen A 5640C 10000 Black PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: SABIC® Vestolen A 5640C 10000 is a grade which has a high density and a bimodal distribution of the molecular mass. It offers a good processability and high stress cracking resistance (ESCR). SABIC® Vestolen A 5640C 10000 is typically used for the coating of steel pipes as part of a three-layer PE system. The product is not intended for and must not be used in any pharmaceutical/medical application.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³ISO 1183
ESCR 10% Igepal® >= 2000 hour>= 2000 hourCO-630, F50; ASTM D1693B
Carbon Black Loading >= 2.0 %>= 2.0 %ISO 6964
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ISO 868
Tensile Strength, Yield 21.0 MPa3050 psiISO 527-2
Elongation at Break >= 600 %>= 600 %ISO 527-2
Elongation at Yield 15 %15 %ISO 527-2
Tensile Modulus 0.850 GPa123 ksiISO 527-2
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 110 °C>= 230 °Fat 10 N (VST/A); ISO 306
 
Descriptive Properties
ColorBlack
RAL number9004

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11113 / 244580

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.