MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Firelite 20XL Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Insulating Aggregate raw material base. Hydraulic bond. A family of really light weight insulating concretes for applications requiring low thermal conductivity coupled with good strength as called for in various areas such as radiant and convection zones, doors etc. of heaters in the petrochemical industry where temperatures up to 1230°C/2250°F may be encountered. The light insulating concrete Firelite 20 may be cast or gunned. The light insulating concretes Firelite 20X and 20XL have separate gunning versions. All of these materials conform to classes N, O and P of ASTM classification C-401-84.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.850 g/cc0.0307 lb/in³dried to 110°C
Grain Size <= 8000 µm<= 8000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.00 MPa290 psiCold Crushing Strength, MST
 2.00 MPa
@Treatment Temp. 1000 °C
290 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 2.10 MPa
@Treatment Temp. 815 °C
305 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 2.90 MPa
@Treatment Temp. 110 °C
421 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.150 W/m-K
@Temperature 200 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.170 W/m-K
@Temperature 400 °C
1.18 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.200 W/m-K
@Temperature 600 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.220 W/m-K
@Temperature 800 °C
1.53 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air <= 1230 °C<= 2250 °F
Shrinkage 0.60 %0.60 %MST
 0.20 %
@Treatment Temp. 815 °C
0.20 %
@Treatment Temp. 1500 °F
 0.30 %
@Treatment Temp. 1000 °C
0.30 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37.1 %37.1 %
CaO 21.3 %21.3 %
Fe2O3 6.7 %6.7 %
K2O+Na2O 1.7 %1.7 %Na2O + K2O
SiO2 31 %31 %
TiO2 1.2 %1.2 %
 
Descriptive Properties
Net Material Required (kg/m³)770

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6380 / 203164

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.