Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processing Method: Injection Molding Forms: Pellets Additive: Heat Stabilizer Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure; High; Injection Rate: Fast Information Provided by Teknor Apex |