MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Elvacite® 4044 Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Elvacite® 4044 is a solid bead resin is a medium molecular weight butyl methacrylate-methyl methacrylate copolymer. It is a relatively soft and flexible acrylic resin for use in manufacture of ceramic covercoats and heat seal lacquers. Elvacite® 4044 is an inherently soft polymer and may block or cake under certain storage conditions. This product should be stored and used at temperatures not exceeding 30°C. If stored under these conditions, lumps may form which may need increased mechanical effort to break down. This does not detract from the performance of the product. It has good compatibility with many binders and plasticisers, and has excellent solubility in a wide range of solvents.

Information provided by Lucite International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1500 - 2000 cP1500 - 2000 cP40% w/w in Shellsol A
Viscosity Test 55 cm³/g0.55 dl/greduced viscosity, 1 wt% in chloroform; Ubbelohde B Viscometer
Molecular Weight 12000 g/mol12000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.000.00
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 32.0 °C89.6 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUCIT9477 / 150191

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.