MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ipiranga Petrochem GM 5250 OC HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.

To produce HDPE, IPQ employs Hoechst/Hostalen technology through the following steps: the ethene supplied by COPESUL is processed by Ipiranga Petroquímica in reactors to produce powdered polyethylene. The polyethylene then receives additives and is homogenized with stabilizers and taken to extruding presses where it is granulated and is ready for marketing.

An integrated and computerized system controls the production, from the initial processing stages to end-product testing for later commercialization.

Applications:

  • corrugated pipe for sewer
  • pipe for streets and roads drainage
  • pipe for drainage in general

Ipiranga Petrochem polymer product lines have been acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 - 0.954 g/ccASTM D792-98
Melt Flow 0.15 - 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238-00
High Load Melt Index 14 - 24 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238-00
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.0 MPaASTM D638-02
Elongation at Yield 8.7 %ASTM D638-02
Flexural Modulus 0.910 GPa
@Strain 2 %
Secant; ASTM D790-02
Izod Impact, Notched 140 J/mASTM D256-03

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem INSPIRE™ 137 NA Performance Polypropylene Polymer
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection
Ascend Performance Materials Starflam® M10009AP PP, Flame Retardant, Injection Molding
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend

PIPIRA22 / 48355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.