MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Biomerics Elast-Eon™ E2-862 Aromatic Polyether Silicone Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: The Elast-Eon™ family of polymers combines the advantageous properties of both polyurethanes and silicone rubbers into a single material. These materials exhibit the physical and mechanical performance of polyurethanes and a biological stability that surpasses rigid biostable polyurethanes. Elast-Eon™ polymers are widely accepted as being the most biostable of all polyurethane materials and as such are being used in long-term implantation. Elast-Eon™ may be used in applications including:
  • CRM Devices (e.g. Pacemaker)
  • Neurostimulation Devices
  • Electro Signaling Devices
  • Breast Implants
  • IUDs
  • Implantable Joint Interface Coating
  • Stents
  • Ear Tubes
  • Heart Wall Graft

Information provided by Biomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868
Tensile Strength at Break 34.0 MPa4930 psi
Elongation at Break >= 200 %>= 200 %
Modulus of Elasticity 0.650 GPa94.3 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 - 215 °C410 - 419 °F
 
Descriptive Properties
Physical FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIOMC088 / 250964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.