MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mafic Chopped Basalt Fiber for Concrete
Categories: Ceramic; Other Engineering Material; Composite Fibers

Material Notes:

Information provided by Mafic Basalt

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filament Diameter 9.0 - 19 µmMay be specified
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 10 %[±10% w/w]
 
Descriptive Properties
Alkali Weight Loss1.4% LosspH 11 NaOH
 2.2% LosspH 11 Na2CO3
Available Chop Fiber Lengths3, 6, 12, 24, 48, 96 mm
Fiber Diameter9 to 19 µm
Fiber TypeBasalt
Sizing Content0.25%[±10% w/w]
Sizing TypeSilane AR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mafic Assembled Basalt Roving 300 to 2000 Tex
Mafic Chopped Basalt Fiber for Resin Reinforcement
Hanwha Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
Glass Fiber Reinforced Concrete

EMAFC004 / 187065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.