MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.

Advantages & Application Notes:

  • Low viscosity epoxy with excellent handling characteristics. It can be used for encapsulating or potting. It may be applied by hand, pouring, spin coating, brushing, dipping, or automated dispensers.
  • Complies with USP Class VI biocompatibility standards.
  • Passes NASA low outgassing standard ASTM E595 with proper cure
  • Suggested Medical Applications / Scientific OEM:
    • Potting fiber ferrules for endoscopes
    • Outstanding high temperature properties at 300°C and excellent solvent, chemical and moisture resistance, including autoclave, ETO, and gamma radiation
  • Suggested Semiconductor Grade epoxy
  • Spin coating at wafer level for MEMS fabrication of pressure sensors and accelerometers
  • Wafer-to-wafer bonding in CSP
  • Capillary underfill of flip chip packaged die
  • Suggested Optical grade epoxy, opto-electronic packaging
  • Transmission in NIR from 700 – 900 nm >95%
  • Glass seal, hermetic seal of glass plates in LCD fabrication
  • Hermetic seal of IR-filter window to aluminum cap of TO-Can in hybrid packaged IR sensors.
  • Suggested Industrial: resist salt water, hydraulic fluids, motor oil, alcohol, 10% nitric acid, 10% sulfuric acid, 10% ammonia solution and most solvents.

    Information Provided by Epoxy Technology

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.15 g/ccPart A
     1.22 g/ccPart B
    Viscosity 150 - 300 cP
    @Temperature 23.0 °C
    100 rpm
     
    Chemical PropertiesOriginal ValueComments
    Ionic Impurities - Na (Sodium) 15 ppm
    Ionic Impurities - K (Potassium) 3.0 ppm
    Ionic Impurities - Cl (Chloride) 26 ppm
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 67
    Tensile Modulus 374000 psiStorage
    Shear Strength 1456 psiLap
     >= 3400 psiDie
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity >= 1.00e+13 ohm-cm
    Dielectric Constant 3.36
    @Frequency 1000 Hz
    Dissipation Factor 0.0050
    @Frequency 1000 Hz
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 57.0 µm/m-°CBelow Tg
     210 µm/m-°CAbove Tg
    Maximum Service Temperature, Air 200 °CContinuous
     300 °CIntermittent
    Minimum Service Temperature, Air -55.0 °CContinuous
     -55.0 °CIntermittent
    Glass Transition Temp, Tg >= 95.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
    Decomposition Temperature 375 °CDegradation Temperature
     
    Optical PropertiesOriginal ValueComments
    Refractive Index 1.5195
    @Wavelength 589 nm
    Transmission, Visible >= 95 %
    @Wavelength 1000 - 1500 nm
    Spectral
     >= 99 %
    @Wavelength 600 nm
    Spectral
     
    Processing PropertiesOriginal ValueComments
    Cure Time 1.00 hour
    @Temperature 150 °C
    Minimum Bond Line
    Pot Life 1440 min
    Shelf Life 12.0 Month
    @Temperature 25.0 °C
     
    Compliance PropertiesOriginal ValueComments
    USP Class VI Yes
     
    Descriptive Properties
    ColorAmberPart B
     Clear/ColorlessPart A
    ConsistencyPourable liquid
    Ionic Impurities NH422 ppm
    Mix Ratio by Weight1:1
    Number of ComponentsTwo
    Weight Loss0.06%200°C
     0.17%250°C
     0.5%300°C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
    Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
    Epoxy Technology EPO-TEK® 375 High Temperature Epoxy
    Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
    Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy

    PPOXYT132 / 141171

    USP Class VI Adhesives
    USP Class VI Approved Adhesives for Medical Device Applications
    Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.