MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: 30% carbon fiber, low melt flow for extrusion and injection molding

AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of the desirable high performance attributes of carbon fiber reinforced PEEK. Those attributes include chemical resistance, fatigue resistance, and long term thermal oxidative stability.

The excellent balance of properties of AV-722 CF30 makes this grade well suited for a broad range of applications across a number of industries, including healthcare, transportation, electronics, oil and gas and chemical processing.

The melt processing behavior of AV-722 CF30 is overall very similar to that of 30% CF reinforced PEEK.

Markets/Uses: Automotive / Mechanical & Structural Parts / Gears

Applications: Automotive Applications; Gears; Industrial Applications

Features: Chemical Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Injection notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 470 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow <= 0.0020 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 107ASTM D785
Tensile Strength 200 MPa5.0 mm/min; ASTM D638
Tensile Strength, Yield 224 MPaType 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.5 %5.0 mm/min; ASTM D638
 1.5 %Type 1A, 5 mm/min; ISO 527-2
Tensile Modulus 22000 MPa5.0 mm/min; ASTM D638
 26600 MPa1 mm/min, Type 1A; ISO 527-2
Flexural Strength 304 MPaASTM D790
 334 MPaISO 178
Flexural Modulus 19300 MPaASTM D790
 25000 MPaISO 178
Compressive Strength 170 MPaASTM D695
Poissons Ratio 0.44ASTM E132
Shear Strength 98.0 MPaASTM D732
Izod Impact, Notched 53.0 J/mASTM D256
Izod Impact, Unnotched 530 J/mASTM D256
Izod Impact, Notched (ISO) 8.50 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 39.0 kJ/m²ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 6.00 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
Specific Heat Capacity 1.28 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.74 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.340 W/m-KASTM C177
Melting Point 340 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 276 °CAnnealed; ASTM D648
Glass Transition Temp, Tg 150 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 366 °C
Middle Barrel Temperature 371 °C
Front Barrel Temperature 377 °C
Nozzle Temperature 382 °C
Mold Temperature 177 - 204 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4155 / 279955

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.