MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials HiDura™ LUX H3X NT0853 Nylon PA 6I/6T Copolymer
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: HiDura LUX H3X NT0853 is a polyamide 6I/6T copolymer grade. It can be used for film applications to enhance processability, shrink, and thermoforming characteristics.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³DAM; ISO 1183
Water Absorption 0.70 %
@Temperature 23.0 °C,
Time 86400 sec
0.70 %
@Temperature 73.4 °F,
Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 2.0 %2.0 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 2.00 mm
0.0060 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 2.00 mm
0.0060 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50% RH; ISO 527-2
 76.0 MPa11000 psiDAM; ISO 527-2
Tensile Strength, Yield 95.0 MPa13800 psi50% RH; ISO 527-2
 99.0 MPa14400 psiDAM; ISO 527-2
Elongation at Break >= 50 %>= 50 %DAM; ISO 527-2
 >= 50 %>= 50 %50% RH; ISO 527-2
Elongation at Yield 5.5 %5.5 %50% RH; ISO 527-2
 8.4 %8.4 %DAM; ISO 527-2
Tensile Modulus 2.80 GPa406 ksi50% RH; ISO 527-2
 3.00 GPa435 ksiDAM; ISO 527-2
Flexural Strength 98.0 MPa14200 psiDAM; ISO 178
 98.0 MPa14200 psi50% RH; ISO 178
Flexural Modulus 3.10 GPa450 ksiDAM; ISO 178
 3.10 GPa450 ksi50% RH; ISO 178
Poissons Ratio 0.380.38ISO 527-2
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 26.0 kV/mm
@Thickness 1.00 mm
660 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 69.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
38.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
37.8 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FUnannealed, 50% RH; ISO 75-2/B
 120 °C248 °FUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FUnannealed, 50% RH; ISO 75-2/A
 110 °C230 °FUnannealed, DAM; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 220 - 240 °C428 - 464 °FExtrusion
 240 - 270 °C464 - 518 °FExtrusion
 240 - 270 °C464 - 518 °FExtrusion
 240 - 270 °C464 - 518 °FExtrusion
 240 - 270 °C464 - 518 °FExtrusion
Die Temperature 250 - 275 °C482 - 527 °FExtrusion
Melt Temperature 240 - 270 °C464 - 518 °FExtrusion
 
Descriptive Properties
Agency RatingsASTM, D4066 PA0000B6405
 ASTM, D6779 PA0000B6405
 ISO, 1043 PA6I6T
AppearanceNatural Color
FeaturesChemical Resistant
 Copolymer
 High Melt Strength
 High Viscosity
FormsPellets
Processing MethodBlow Molding
 Film Extrusion
 Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8602 / 293351

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.