MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmodur® E 14 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Aromatic polyisocyanate prepolymer based on toluene diisocyanate. In the formulation of highly flexible coatings, sealers and two-component PU sealing compounds.

Properties / Applications: Desmodur® E 14 can be combined with Hardener® DT to formulate highly flexible sealers. Used in one-component PU formulations, Desmodur® E 14 will improve flexibility.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccDIN EN ISO 2811-1
Viscosity 5600 - 8000 cP5600 - 8000 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesMetricEnglishComments
Flash Point 200 °C392 °FDIN EN ISO 2719
 
Descriptive Properties
Color<2Iodine, DIN EN 1557
Content<0.5%Monomeric HDI, DIN EN ISO 10283
 3.1-3.5%NCO, DIN EN ISO 11909

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmodur® BL 1100/1 Polyurethane
Covestro Desmodur® E 1160 MPA/X Polyurethane
Covestro Desmodur® E 15 Polyurethane
Covestro Desmodur® E 21 Polyurethane
Covestro Desmodur® E 210 Polyurethane

PCOVEST0335 / 202118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.