Notes: 235G is a 35% glass fiber reinforced nylon 6 that offers a balance between mechanical performance, surface finish and mold release characteristics. Availability: Europe Fillers/Reinforcement: Glass Fiber, 35% Filler by Weight Processing Method: Injection Molding Information provided by Teknor Apex |