MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Mylar® M461 Polyester Film, 75 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX film type.

Mylar® M461 has balanced tensile properties and excellent resistance to moisture and most chemicals. It can withstand temperature extremes from -94 to 302°F. Mylar® M461 does not become brittle with age under normal conditions because it does not contain plasticizers.

Typical Applications: Mylar® M461 film is used primarily as a base for pressure sensitive tapes.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccTypical Mylar®; ASTM D1505
Thickness 0.750 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 115 %ASTM D882A
Film Tensile Strength at Break, MD 25000 psiASTM D882A
Film Tensile Strength at Break, TD 33000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.17 J/g-°CTypical Mylar®
Melting Point 254 °CTypical Mylar® via DSC
Maximum Service Temperature, Air 302 °F
Minimum Service Temperature, Air -94.0 °F
Shrinkage, MD 2.3 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD 0.70 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64 - 1.67typical of Mylar®
Haze 5.0 %ASTM D1003
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 75 Gauge
DuPont Teijin Films Mylar® 75 OL Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® P25T Polyester Film, 75 Gauge
DuPont Teijin Films Mylar® P25 Polyester Film, 75 Gauge

PDTZ9352 / 139672

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.