MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Durabond® E-00CL Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes:
Epoxy Adhesives
Loctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 application-specific products designed to outperform the competition in all aspects: better adhesion, better flow, less odor, improved clarity, higher strength, and greater durability. All two-part Durabond® Structural Adhesives are packaged in easy-to-use, side-by-side cartridges for use with our manual dispensers and mix nozzles.

Loctite® E-00CL Fast setting, flowable, low odor Durabond® Epoxy Adhesive
A fast setting epoxy with a 5-minute worklife. Clear, flowable, low-odor.
  • Mix Ratio by Volume, Resin:Hardener = 1:1
Bonding Type: Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 9300 cPMixed - low; Resin - 9,300 cP; Hardener - 2,700 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Adhesive Bond Strength 2000 - 4000 psiVaries with substrates
Peel Strength 1.00 - 5.00 pliVaries with substrates.
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/milTest run on 1/8" specimens.
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 20.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 3.0 - 5.0 min
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Durabond® E-214HP Epoxy Adhesive
Henkel Loctite® 3888 Room Temperature Cure Isotropic Epoxy Adhesive
Henkel Loctite® 3335 Epoxy Light Cure Adhesive
Henkel Loctite® Durabond® M-21HP Epoxy Adhesive
Henkel Loctite® Durabond® E-20NS Epoxy Adhesive

PLOCT045 / 51781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.