Notes: Monprene CP-28128 X4 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP--28128 X4 is a low hardness, low density grade that exhibits excellent melt strength and flexibility characteristics. This grade is suitable for injection molding or extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Melt Strength; Good Moldability; Good Processability; Good Tear Strength; Good Toughness; Halogen Free; High Elongation; High Tensile Strength; Low Compression Set; Low Density; Low Hardness; Low Flow; Lubricated; Resilient Uses: Flexible Grips; Foam; Gaskets; General Purpose; Handles; Hose; Knobs; Profiles; Rubber Replacement; Seals; Tubing; Windows & Doors RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion; Cast Film Information provided by Teknor Apex |