Reinforced with 15% of glass fiber and modified polyamide 66, with improved impact resistance, heat stabilized for injection molding. Eplamid 66 GFI 15 is used in all sectors of industry, offering a good impact strength for mechanical properties, ensures outstanding performance even at low temperatures.Information provided by Epsan Plastik |