MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Ultrathene® UE672102 Ethylene Vinyl Acetate Copolymer, Film Grade
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as well as liquid and heavy duty packaging and pallet stretch film. UE672 contains antioxidant and high levels of slip and antiblock additives.

Regulatory Status: UE672 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows for the use of this material in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques: The maximum recommended melt temperature for UE672 is 430°F (221°C).

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 85.3 g/m²/dayASTM F372
Oxygen Transmission Rate 8900 cc/m²/dayASTM D3985
Vinyl Acetate Content 13.5 %
Thickness 1.50 mil
Melt Flow 0.50 g/10 minASTM D1238
Antiblock Level 6300 ppm
Slip Level 2100 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 960 psiASTM D882
Film Tensile Strength at Yield, TD 800 psiASTM D882
Film Elongation at Break, MD 300 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
Film Elongation at Yield, MD 18 %ASTM D882
Film Elongation at Yield, TD 16 %ASTM D882
Elmendorf Tear Strength MD 92 gASTM D1922
Elmendorf Tear Strength TD 128 gASTM D1922
Dart Drop 380 g/milASTM D4272
Film Tensile Strength at Break, MD 4430 psiASTM D882
Film Tensile Strength at Break, TD 4320 psiASTM D882
1% Secant Modulus, MD 13100 psiASTM D882
1% Secant Modulus, TD 13200 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 80.0 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 1.5 %ASTM D1003
Gloss 88 %45°; ASTM D2457
Transmission, Visible 78 %NAS; ASTM D1746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 420 °F
Die Opening 0.0635 cm
Blow-up Ratio (BUR) 2.0
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045.11 Linear Low Density Polyethylene, Heavy Duty Film Grade
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade
LyondellBasell Ultrathene® UE624000 Ethyl Vinyl Acetate Copolymer
LyondellBasell Ultrathene® UE672006 Ethylene Vinyl Acetate Copolymer, Film Grade
Versalis Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion

PEQU0808 / 104164

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.