MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Electrolytic Copper Tough Pitch, hot forged rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.7 µm/m-°C
@Temperature -4.00 - 149 °C
9.83 µin/in-°F
@Temperature 24.8 - 300 °F
Thermal Conductivity 392 W/m-K2720 BTU-in/hr-ft²-°F
Melting Point 1083 °C1981 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 99.9 %99.9 %
Other 0.060 %0.060 %
Oxygen, O 0.040 %0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Electrolytic Copper Tough Pitch, strip 427°C (800°F) anneal for 1 hour
Electrolytic Copper Tough Pitch, 50% hard-drawn rod
Electrolytic Copper Tough Pitch, cold forged 40% cold reduction rod
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Electrolytic Copper Tough Pitch, 538°C (1000°F) annealed rod

MMCUA3 / 12352

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.