MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® RG-17270 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-17200 series is a group of high performance thermoplastic elastomers specifically designed for EU injection molded regulated applications including food contact, toys, and children’s products. Monprene RG-17270 is a medium density, medium hardness grade that complies with various US FDA and European regulations and directive for food contact and toy safety and is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Medium Density; Medium Hardness; Lubricated

Uses: Closures; Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Gaskets; Handles; Kitchenware; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Viscosity 109 cP
@Shear Rate 206 1/s,
Temperature 200 °C
109 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ISO 11443
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  70
@Time 5.00 sec
70
@Time 0.00139 hour
ISO 868
 72
@Time 1.00 sec
72
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 8.27 MPa1200 psiISO 37
Tensile Stress at Strain  2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
ISO 37
 2.40 MPa
@Strain 300 %
348 psi
@Strain 300 %
ISO 37
Elongation at Break 700 %700 %ISO 37
Compression Set  34 %
@Temperature 22.8 °C,
Time 79200 sec
34 %
@Temperature 73.0 °F,
Time 22.0 hour
Method B; ISO 815
 55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
Method B; ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 120 - 160 °C248 - 320 °F
Middle Barrel Temperature 160 - 230 °C320 - 446 °F
Front Barrel Temperature 180 - 230 °C356 - 446 °F
Nozzle Temperature 180 - 230 °C356 - 446 °F
Melt Temperature 180 - 230 °C356 - 446 °F
Mold Temperature 15.0 - 50.0 °C59.0 - 122 °F
Back Pressure 0.500 - 1.50 MPa72.5 - 218 psi
Cushion 0.300 - 2.00 cm0.118 - 0.787 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0929 / 237420

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.